聚丙烯儲罐的襯膠方式

瀏覽量

  隨著時代的不斷發展,聚丙烯儲罐這個詞也越來越被人們熟知,目前,很多儲罐為了便于物品的輸送,在儲存重油和原油的罐內設有加熱器,我們的聚丙烯儲罐外側也要采取保溫措施,便是它的襯膠方式。

  對于聚丙烯儲罐直徑小于6米或長度短于15米的部件一般采用車間襯膠。具體指部分管件、管道、懸浮液的噴淋裝置、吸收塔內的其他不同小構件。工藝:車間內,部件先被鋪上未硫化過的橡膠板,然后在壓熱硫化釜內,溫度120℃-150℃、壓力6巴下進行硫化。橡膠襯里大部分采用現場襯膠。現場襯膠使用在車間內預硫化的橡膠板以及自硫化的橡膠板,現場進行粘和,不過采用前者多于后者。由于丁基橡膠需要較高的硫化溫度,所以一般丁基橡膠的襯膠在車間內完成。

  聚丙烯儲罐的襯膠還有一個優點:就是對軟弱地基要嚴格控制充水速率,使罐體的沉降不致太快,同時要注意罐體四周的地表土的變化,避免地基剪切破壞。

 

With the continuous development of the times, the term polypropylene tank is more and more well known. At present, many storage tanks have heaters in tanks for storing heavy oil and crude oil for the convenience of goods transportation. The insulation measures on the outside of our polypropylene tank are also adopted, that is, its lining method.
Workshop lining is generally used for parts with diameter less than 6 meters or length less than 15 meters of polypropylene tank. Specifically refers to some pipe fittings, pipelines, suspension spraying device, other different small components in absorption tower. Process: In the workshop, the parts are first covered with unvulcanized rubber sheets, and then vulcanized in the autoclave under pressure of 6 bars and temperature of 120 - 150 degrees Celsius. Rubber lining mostly uses on-site lining. Field lining is made of pre-vulcanized rubber sheets and self-vulcanized rubber sheets in the workshop, which are bonded on site, but the former is more than the latter. Because butyl rubber needs a higher vulcanization temperature, the general butyl rubber lining is completed in the workshop.
Another advantage of polypropylene tank lining is that the filling rate of soft foundation should be strictly controlled so that the settlement of the tank can not be too fast. At the same time, the change of surface soil around the tank should be noticed to avoid the shear failure of the foundation.